PSC is made from about 31% clinker, up to 65% ground granulated blast furnace slag (GGBFS) and 4% gypsum. Like PPC, it gives more durable concrete than OPC, especially in mass concreting and aggressive conditions.
Compressive strength
| Age | DCCL target | Standard minimum |
|---|---|---|
| 3 days | 23 MPa | 16 MPa |
| 7 days | 33 MPa | 22 MPa |
| 28 days | 43 MPa | 33 MPa |