OPC 43 is made by grinding clinker with about 4% gypsum. It sets quickly and develops high early strength, reaching at least 43 MPa (430 kg/cm²) at 28 days.
Compressive strength
| Age | DCCL target |
|---|---|
| 3 days | 23 MPa |
| 7 days | 33 MPa |
| 28 days | 43 MPa |

OPC
Sets fast and gains strength early. For structural concrete, roads, bridges, runways and work where formwork must come off quickly.
OPC 43 is made by grinding clinker with about 4% gypsum. It sets quickly and develops high early strength, reaching at least 43 MPa (430 kg/cm²) at 28 days.
| Age | DCCL target |
|---|---|
| 3 days | 23 MPa |
| 7 days | 33 MPa |
| 28 days | 43 MPa |